Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 3.38 MPa | 490 psi | |
BCC Products DP-11-83 Urethane Adhesive-Slo DP-11-83 is a low viscosity, quick setting, easy to use adhesive and/or casting material. This product was designed to bond together the MB1200 foam board to create desired dimensions in length, wid.. |
|||
Tensile Strength, Ultimate | 3.38 MPa | 490 psi | Across Flow; ASTM D412 |
ExxonMobil Santoprene® 111-73 Thermoplastic Elastomer
(discontinued **) A soft, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide range .. |
|||
Tensile Strength, Ultimate | 3.38 MPa | 490 psi | Across Flow; ASTM D412 |
ExxonMobil Santoprene® 121-80M300 Thermoplastic Elastomer
(discontinued **) A soft, black, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material is designed for automotive interior applications requiring low fogging and good.. |
|||
Tensile Strength, Ultimate | 3.38 MPa | 490 psi | Across Flow; ASTM D412 |
ExxonMobil Santoprene® 211-73 Thermoplastic Elastomer
(discontinued **) A soft, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ra.. |