Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 28.42 - 60.0 MPa @Temperature 70.0 - 100 °C |
4122 - 8700 psi @Temperature 158 - 212 °F |
Average value: 46.5 MPa Grade Count:6 |
Overview of materials for Thermoplastic Polyurethane, Elastomer, Ether Grade This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane, Elastomer, Ether Grade". Each property range of values reported is minimum a.. |
|||
Tensile Strength, Ultimate | 28.42 - 60.0 MPa @Time 0.000 - 4.84e+6 sec |
4122 - 8700 psi @Time 0.000 - 1340 hour |
Average value: 46.5 MPa Grade Count:6 |
Overview of materials for Thermoplastic Polyurethane, Elastomer, Ether Grade This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane, Elastomer, Ether Grade". Each property range of values reported is minimum a.. |