Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 17.3 MPa

@Thickness 3.17 mm
2510 psi

@Thickness 0.125 in
Type IV specimen, 2" per minute test speed, rotomolded samples; ASTM D638
NOVA Chemicals Novapol® TR-0735-U Hexene MDPE Rotational Molding Resin
Good impact resistance, Excellent processabilityApplications: Toys, Complex custom parts, Home and garden items, MailboxesAdditives: Processing antioxidants, UV stabilizersInformation provided by NO..
Tensile Strength, Ultimate 17.3 MPa

@Thickness 3.17 mm
2510 psi

@Thickness 0.125 in
Type IV specimen, 2" per minute test speed, rotomolded samples; ASTM D638
NOVA Chemicals Novapol® PR-0636-UG Butene MDPE Rotational Molding Resin  (discontinued **)
Very good processability, Very good ESCR, Good impact properties, NSF listed for Stds. 14, 24, and 61Applications: Toys, General purpose custom molding, Carts, Playground equipmentAdditives: Process..
Tensile Strength, Ultimate 17.3 MPa

@Thickness 3.17 mm
2510 psi

@Thickness 0.125 in
Type IV specimen, 2" per minute test speed, rotomolded samples; ASTM D638
NOVA Chemicals Sclair® TD-7915-UG Hexene MDPE Rotational Molding Resin  (discontinued **)
Excellent low temperature impact properties, Excellent ESCR, Wide process window, NSF listing for Stds. 14, 24, and 61 pending, Retention of impact at long cook timesApplications: IBCs, Toys, Genera..
Tensile Strength, Ultimate 17.3 MPa
2510 psi
DuPont Vamac® GXF Sample Compound Vulcanizate Slab Cure (5 minutes at 190°C) Without Armeen® 18D
Test slab is cured for 5 minutes at 190°C and post cured for 4hrs at 175°C. Vulcanizate performance test data can help end-users evaluate the potential fitness of similar compounds for their own ..
Tensile Strength, Ultimate 17.3 MPa

@Thickness 3.17 mm
2510 psi

@Thickness 0.125 in
Type IV specimen, 2" per minute test speed, rotomolded samples; ASTM D638
NOVA Chemicals Sclair® TD-7915-U Hexene MDPE Rotational Molding Resin  (discontinued **)
Excellent low temperature impact properties, Excellent ESCR, Wide process window, NSF listing for Stds. 14, 24, and 61 pending, Retention of impact at long cook timesApplications: IBCs, Toys, Genera..
Tensile Strength, Ultimate 17.3 MPa

@Thickness 3.17 mm
2510 psi

@Thickness 0.125 in
Type IV specimen, 2" per minute test speed, rotomolded samples; ASTM D638
NOVA Chemicals Novapol® PR-0636-U Butene MDPE Rotational Molding Resin  (discontinued **)
Very good processability, Very good ESCR, Good impact properties, NSF listed for Stds. 14, 24, and 61Applications: Toys, General purpose custom molding, Carts, Playground equipmentAdditives: Process..