Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 1700 MPa | 247000 psi | Typical |
Industeel FORA 500 500 HB Wear Resistant Steel Description: FORA 500 is a water quenched martensitic steel, with a 500HB (51.5 HRC), typical hardness, resistant to very severe abrasion wear. Thanks to its mechanical properties, good toughness, h.. |
|||
Tensile Strength, Ultimate | 1700 MPa @Thickness 25.4 mm |
247000 psi @Thickness 1.00 in |
filament |
3M Nextel™ 312 Industrial Ceramic Fiber Chemical composition above is wt%. Crystal phase is mullite + amorphous (or 100% amorphous). Filament diameter is 10-12 µm.3M Nextel fibers 312, 440, and 550 are designed for non-structural appli.. |