Material Notes:
Chemical composition above is wt%. Crystal phase is mullite + amorphous (or 100% amorphous). Filament diameter is 10-12 µm.3M Nextel fibers 312, 440, and 550 are designed for non-structural applications where their primary purpose is to act as a flame barrier. 3M Nextel Ceramic Fiber 312 is made from Al2O3, SiO2, and B2O3. Because B2O3 is present, this composition has both crystalline and glassy phases. The glassy phase helps the fiber retain strength after exposure to high temperatures because it slows the growth of crystalline phases that weaken the fiber. However, when the fiber is stressed at high temperature, the glassy phase weakens the fiber due to viscous flow much like a glass fiber.Information provided by 3M Ceramic Textile and Composites.
Physical Properties Metric English Comments
Density 2.70 g/cc
0.0975 lb/in³
Particle Size <= 0.50 µm
<= 0.50 µm
Crystal size
Specific Surface Area <= 0.20 m²/g
<= 0.20 m²/g
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 1700 MPa

@Thickness 25.4 mm
247000 psi

@Thickness 1.00 in
filament
Modulus of Elasticity 150 GPa
21800 ksi
Filament in Tension
Thermal Properties Metric English Comments
CTE, linear 3.00 µm/m-°C

@Temperature 25.0 - 500 °C
1.67 µin/in-°F

@Temperature 77.0 - 932 °F
Specific Heat Capacity 1.05 J/g-°C

@Temperature 500 °C
0.251 BTU/lb-°F

@Temperature 932 °F
Melting Point 1800 °C
3270 °F
Optical Properties Metric English Comments
Refractive Index 1.568
1.568
Component Elements Properties Metric English Comments
Al2O3 62.5 %
62.5 %
B2O3 13 %
13 %
SiO2 24.5 %
24.5 %
Electrical Properties Metric English Comments
Dielectric Constant 5.2

@Frequency 9.375e+9 Hz
5.2

@Frequency 9.375e+9 Hz
Dissipation Factor 0.018

@Frequency 9.375e+9 Hz
0.018

@Frequency 9.375e+9 Hz
Descriptive Properties Value Comments
Color White
Users viewing this material also viewed the following: