Polymer Property : Tensile Strength, Ultimate = 23400.0 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 9.00 - 161.337 MPa

@Temperature -40.0 - 120 °C
1310 - 23400.0 psi

@Temperature -40.0 - 248 °F
Average value: 69.4 MPa Grade Count:3
Overview of materials for High Density Polyethylene (HDPE), Glass fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Glass fiber Filled". Each property range of values reported is minimum..