Tensile Strength, Ultimate 1240 - 1520 MPa
180000 - 220000 psi
Materion Beryllium Copper Alloy 25 Plate & Rolled Bar; HT (TH04) Temper; over 9.5 to 25 mm Thickness (UNS C17200)
Treatment required for max strength: 2 hrs @ 330°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials In..
Tensile Strength, Ultimate 1240 - 1520 MPa
180000 - 220000 psi
Materion Beryllium Copper Alloy 25 Rod and Bar; HT (TH04) Temper; over 9.5 to 25.4 mm (UNS C17200)
Treatment required for max strength: 2-3 hrs @ 315-330°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materi..
Tensile Strength, Ultimate 1310 - 1520 MPa
190000 - 220000 psi
Materion Beryllium Copper Alloy 25 Strip; HT (TH04) Temper (UNS C17200)
Treatment required for max strength: 2 hrs @ 315ºCStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 98%Stress Relaxation after 1000 hrs @ 200°C: 74%Superficial Hardness: 30N 58-6..
Tensile Strength, Ultimate 1240 - 1520 MPa
180000 - 220000 psi
Materion Beryllium Copper Alloy 25 Tube; HT (TH04) Temper; over 9.5 to 25.4 mm o.d. (UNS C17200)
Treatment required for max strength: 2-3 hrs @ 315-330°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materi..
Tensile Strength, Ultimate 1240 - 1520 MPa
180000 - 220000 psi
Materion Beryllium Copper Alloy M25 Rod and Bar; HT (TH04) Temper; over 9.5 to 25.4 mm (UNS C17300)
Treatment required for max strength: 2-3 hrs @ 315-330°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materi..