Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | >= 1482 MPa | >= 214900 psi | |
Materion Beryllium Nickel Strip - Alloy 360 Annealed, 2.5 hr at 950°F Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: 2.5 hrs @ 510ºCStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 99%Stress Relaxation.. |
|||
Tensile Strength, Ultimate | 1482 MPa | 214900 psi | |
HP Alloys Alloy 718, 10% Cold Worked, Aged 10% Cold Worked, Aged applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc., Allvac, Inco Alloys International, and Haynes Int.. |