Mechanical Properties Metric English Comments
Tensile Strength, Ultimate >= 1482 MPa
>= 214900 psi
Materion Beryllium Nickel Strip - Alloy 360 Annealed, 2.5 hr at 950°F
Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: 2.5 hrs @ 510ºCStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 99%Stress Relaxation..
Tensile Strength, Ultimate 1482 MPa
214900 psi
HP Alloys Alloy 718, 10% Cold Worked, Aged
10% Cold Worked, Aged applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc., Allvac, Inco Alloys International, and Haynes Int..