Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 1450 MPa | 210000 psi | |
Special Metals Nitinol High-Strength Superelastic Ni-Ti alloy Special Metals Corporation is a producer of a series of "Nitinol" and other shape memory alloys used for a range of applications from precision engineering to medical technology. |
|||
Tensile Strength, Ultimate | >= 1450 MPa | >= 210000 psi | |
Special Metals Nitinol High-Strength Superelastic Ni-Ti-Fe alloy Special Metals Corporation is a producer of a series of "Nitinol" and other shape memory alloys used for a range of applications from precision engineering to medical technology. |
|||
Tensile Strength, Ultimate | 1450 MPa | 210000 psi | |
SSAB Tunnplat Domex® 024 BOR Oil quenched Boron Steel Domex® is the brand name of hot rolled products from SSAB Tunnplat. Compared to conventional quenched and tempered steels, boron steel have several benefits including better formability. Boron .. |
|||
Tensile Strength, Ultimate | 1450 MPa | 210000 psi | Typical |
TIMET TIMETAL® 551 (Ti-4Al-4Mo-4Sn-0.5Si) Titanium Alloy; High-Strength Forging AlloyIndustry Specifications: UK Aerospace Specifications BS TA.38, 39, 40, 41, 42.Features: TIMETAL 551 has high strength and is creep resistant up to 400°C. It has a simila.. |
|||
Tensile Strength, Ultimate | 1448 MPa | 210000 psi | |
AK Steel PH 15-7 Mo® Precipitation Hardening Stainless Steel, Condition TH 1050 AK Steel 15-7 Mo® provides high strength and hardness, good corrosion resistance and minimum distortion on heat treatment. It is easily formed in the annealed condition and develops effective bala.. |
|||
Tensile Strength, Ultimate | 1450 MPa @Temperature 204 °C |
210000 psi @Temperature 400 °F |
|
ATI Allvac® 718Plus™ Nickel Superalloy Allvac 718Plus alloy (UNS N07818) is a precipitation hardened nickel-base material that exhibits high temperature tensile strength and stress rupture performance. This alloy is designed to have the.. |
|||
Tensile Strength, Ultimate | 1450 MPa | 210000 psi | |
Carpenter Extendo-Die® Hot Work Die Steel, Tempered 621°C Data provided by Carpenter Technology Corporation.This steel combines extreme toughness with good red hardness in large section sizes. This alloy may also be considered for many cold work applicati.. |
|||
Tensile Strength, Ultimate | 1448 MPa | 210000 psi | |
AK Steel 17-4 PH® Precipitation Hardening Stainless Steel, Condition H 900 AK Steel 17-4 PH® provides an outstanding combination of high strength, good corrosion resistance, good mechanical properties at temperatures up to 600°F (316°C), and good toughness in both base.. |
|||
Tensile Strength, Ultimate | 1450 MPa | 210000 psi | |
Touchstone MetPreg™ Fiber Reinforced Aluminum MetPreg™ is a unique Fiber Reinforced Aluminum (FRA) material, a true metal matrix composite (MMC), that makes use of all traditional composite processing techniques. MetPreg has all the advantages.. |