Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 1410 - 1420 MPa | 205000 - 206000 psi | |
Latrobe Lescalloy® UT-18 VAC-ARC ; 3.25 in. round High Strength Alloy Steel UT-18 VAC-ARC is a medium-carbon, low-alloy heat resistant steel having high strength to 1000°F. It is used primarily for turbine and compressor rotor shafts. Vacuum consumable electrode melting.. |
|||
Tensile Strength, Ultimate | 1410 - 1420 MPa | 204000 - 206000 psi | |
Latrobe Lescalloy® UT-18 VAC-ARC ; 4 in. round High Strength Alloy Steel UT-18 VAC-ARC is a medium-carbon, low-alloy heat resistant steel having high strength to 1000°F. It is used primarily for turbine and compressor rotor shafts. Vacuum consumable electrode melting.. |
|||
Tensile Strength, Ultimate | 1200 - 1420 MPa | 174000 - 206000 psi | |
Materion Beryllium Copper Alloy 25 Strip; 1/4HT (TH01) Temper (UNS C17200) Treatment required for max strength: 2 hrs @ 315ºCStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 96%Stress Relaxation after 1000 hrs @ 200°C: 70%Superficial Hardness: 30N 56-6.. |
|||
Tensile Strength, Ultimate | 1410 - 1420 MPa | 204000 - 206000 psi | |
Latrobe Lescalloy® UT-18 VAC-ARC ; 1.75 in. round High Strength Alloy Steel UT-18 VAC-ARC is a medium-carbon, low-alloy heat resistant steel having high strength to 1000°F. It is used primarily for turbine and compressor rotor shafts. Vacuum consumable electrode melting i.. |