Polymer Property : Tensile Strength, Ultimate = 205 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 1.41 MPa
205 psi
cured 7 days, 25°C; 45-55% RH; ISO 37
Loctite® 5920™ RTV Silicone Sealant
LOCTITE® 5920™ is a moisture-curing, non-corrosive silicone. The thixotropic nature of LOCTITE® 5920™ reduces the migration of liquid product after application to the substrate. It has been desi..