Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 1.41 MPa | 205 psi | cured 7 days, 25°C; 45-55% RH; ISO 37 |
Loctite® 5920™ RTV Silicone Sealant LOCTITE® 5920™ is a moisture-curing, non-corrosive silicone. The thixotropic nature of LOCTITE® 5920™ reduces the migration of liquid product after application to the substrate. It has been desi.. |