Polymer Property : Tensile Strength, Ultimate = 205 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 50.0 - 205 MPa

@Temperature -50.0 - 250 °C
7250 - 29700 psi

@Temperature -58.0 - 482 °F
Average value: 124 MPa Grade Count:1
Overview of materials for Polyaryletherketone (PAEK), Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyaryletherketone (PAEK), Glass Fiber Filled". Each property range of values reported is minimum and m..
Tensile Strength, Ultimate 110 - 205 MPa
16000 - 29700 psi
Average value: 159 MPa Grade Count:7
Overview of materials for Nylon 46, Lubricated + Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 46, Lubricated + Glass Fiber Reinforced". Each property range of values reported is minimum and ma..