Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 9.00 - 140.653 MPa

@Temperature -40.0 - 120 °C
1310 - 20400.0 psi

@Temperature -40.0 - 248 °F
Average value: 58.0 MPa Grade Count:30
Overview of materials for Polypropylene with 30% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 30% Glass Fiber Filler". Specific grades with glass content between 25% and 34% are i..