Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 1379 - 1551 MPa | 200000 - 225000 psi | |
Materion Beryllium Nickel Strip - Alloy 360 MH6, Mill Hardened Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: Mill HardenedStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 99%Stress Relaxation afte.. |
|||
Tensile Strength, Ultimate | 1380 MPa | 200000 psi | 177°C Temper Temperature |
Latrobe Lescalloy® 16NCD13 VAC-ARC High Strength Alloy Steel 16NCD13 VAC-ARC is a premium quality low alloy, carburizing casehardenable vacuum arc remelted steel which takes its name from the French industry designation. In the carburized condition, its high .. |
|||
Tensile Strength, Ultimate | 1380 - 1650 MPa | 200000 - 240000 psi | |
Special Metals DURANICKEL® 301 (UNS N03301) Spring Wire, Aged Tensile strength (ultimate) and elongation values reported here are typical for Spring Wire, Aged specifically. Other property values are typical of aged DURANICKEL® alloy 301 or the alloy in gen.. |
|||
Tensile Strength, Ultimate | 1380 MPa | 200000 psi | |
Elgiloy® Co-Cr-Ni Alloy, Wire, 30% Cold Reduction The strength, shear modulus, and hardness values are specific to this cold reduction treatment; other values below are typical of Elgiloy®.General Elgiloy® information: High strength, ductility, f.. |
|||
Tensile Strength, Ultimate | 1380 MPa | 200000 psi | Fiber Strand |
Cytec Thornel® VCB-20 Carbon Fiber Cloth Data provided by the manufacturer, Amoco Performance Products, Inc.Used as a reinforcement in structural, ablative, and abrasion-resistant composites.2000 filaments/strand, 99+% carbon assayThornel®.. |
|||
Tensile Strength, Ultimate | 1379 MPa | 200000 psi | |
AK Steel 17-4 PH® Precipitation Hardening Stainless Steel, Condition H 925 AK Steel 17-4 PH® provides an outstanding combination of high strength, good corrosion resistance, good mechanical properties at temperatures up to 600°F (316°C), and good toughness in both base.. |
|||
Tensile Strength, Ultimate | 1380 MPa @Temperature 427 °C |
200000 psi @Temperature 800 °F |
|
ATI Allvac® 718Plus™ Nickel Superalloy Allvac 718Plus alloy (UNS N07818) is a precipitation hardened nickel-base material that exhibits high temperature tensile strength and stress rupture performance. This alloy is designed to have the.. |
|||
Tensile Strength, Ultimate | 1379 MPa | 200000 psi | |
ATI Allvac® M-252 Nickel Superalloy, Heat Treatment: 1177°C (2150°F) Anneal Applications: Turbine blades, fasteners, and high temperature bolting.Data provided by Allvac. |
|||
Tensile Strength, Ultimate | 1379 MPa | 200000 psi | |
AK Steel 17-7 PH® Precipitation Hardening Stainless Steel, Condition TH 1050 AK Steel 17-7 PH® provides high strength and hardness, excellent fatigue properties, good corrosion resistance, good formability, and minimum distortion upon heat treatment. This alloy provides va.. |
|||
Tensile Strength, Ultimate | >= 1379 MPa | >= 200000 psi | |
HP Alloys Nitronic® 50 Austenitic Stainless, Level 5 Cold Worked Cold Worked applies to tensile values and are for 0.25 to 1.5 in. diameter samples; other properties are typical of this alloy.Nitronic® 50 Stainless Steel provides a combination of corrosion resis.. |
|||
Tensile Strength, Ultimate | >= 1379 MPa | >= 200000 psi | |
HP Alloys Nitronic® 60 Austenitic Stainless, Level 5 Cold Worked Level 5 Cold Worked applies to tensile properties of 0.25 to 1.5 in. sizes; other properties are typical of this alloy.Nitronic 60 is truly an all purpose metal. This fully austenitic alloy was orig.. |