Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 1380 MPa | 200000 psi | 177°C Temper Temperature |
Latrobe Lescalloy® 16NCD13 VAC-ARC High Strength Alloy Steel 16NCD13 VAC-ARC is a premium quality low alloy, carburizing casehardenable vacuum arc remelted steel which takes its name from the French industry designation. In the carburized condition, its high .. |
|||
Tensile Strength, Ultimate | 1380 - 1650 MPa | 200000 - 240000 psi | |
Special Metals DURANICKEL® 301 (UNS N03301) Spring Wire, Aged Tensile strength (ultimate) and elongation values reported here are typical for Spring Wire, Aged specifically. Other property values are typical of aged DURANICKEL® alloy 301 or the alloy in gen.. |
|||
Tensile Strength, Ultimate | 1380 MPa | 200000 psi | |
Elgiloy® Co-Cr-Ni Alloy, Wire, 30% Cold Reduction The strength, shear modulus, and hardness values are specific to this cold reduction treatment; other values below are typical of Elgiloy®.General Elgiloy® information: High strength, ductility, f.. |
|||
Tensile Strength, Ultimate | 1380 MPa | 200000 psi | Fiber Strand |
Cytec Thornel® VCB-20 Carbon Fiber Cloth Data provided by the manufacturer, Amoco Performance Products, Inc.Used as a reinforcement in structural, ablative, and abrasion-resistant composites.2000 filaments/strand, 99+% carbon assayThornel®.. |
|||
Tensile Strength, Ultimate | 1380 MPa @Temperature 427 °C |
200000 psi @Temperature 800 °F |
|
ATI Allvac® 718Plus™ Nickel Superalloy Allvac 718Plus alloy (UNS N07818) is a precipitation hardened nickel-base material that exhibits high temperature tensile strength and stress rupture performance. This alloy is designed to have the.. |