Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 43.0922 - 1241.06 MPa @Temperature -55.0 - 332 °C |
6250.01 - 180000 psi @Temperature -67.0 - 630 °F |
Average value: 376 MPa Grade Count:14 |
Overview of materials for Polyimide This property data is a summary of similar materials in the MatWeb database for the category "Polyimide". Each property range of values reported is minimum and maximum values of appropriate MatWeb e.. |
|||
Tensile Strength, Ultimate | 552 - 1240 MPa | 80000 - 180000 psi | |
Meehanite Ductliron® AQS Nodular Graphite Ductile Iron Type AQS is an air hardening metal possessing high strength, toughness and hardness. It may be fully air quenched throughout casting section after machining to a wide range of strength and hardness.. |
|||
Tensile Strength, Ultimate | 1070 - 1241 MPa | 155000 - 180000 psi | |
Materion Beryllium Nickel Strip - Alloy 360 MH2, Mill Hardened Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: Mill HardenedStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 99%Stress Relaxation afte.. |
|||
Tensile Strength, Ultimate | 1170 - 1240 MPa | 170000 - 180000 psi | |
Crucible Steel Maxel® 2000 Stainless Steel Maxel 2000 is a free-machining stainless holder block steel which is based on the nominal analysis of Type 414L rather than Type 420. It is supplied pre-hardened to about HRC 37. Due to its unique c.. |