Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 1144 MPa | 165900 psi | |
TIMET TIMETAL® 6-2-4-6 Titanium Alloy (Ti-6Al-2Sn-4Zr-6Mo), 50% Equiaxed Alpha + STOA This entry has UTS, TYS, Elongation, ROA, and fatigue values specific to material in the 50% Equiaxed Alpha + STOA (885°C/1hr/AC + 705°C/1hr/AC) condition. Other data below are typical of TIMETAL.. |
|||
Tensile Strength, Ultimate | 1144 MPa @Temperature -73.0 °C |
165900 psi @Temperature -99.4 °F |
|
Carpenter Gall-Tough PLUS™ Stainless, Annealed, 10% Cold Work Data provided by Carpenter Technology Corporation.Annealed 1150°C, water quenched, and cold drawn.Threshold Galling Stress 48 MPa. The avg. total volume loss on the wear test is 10.6 mm³ at 100 r.. |