Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 11.20 MPa | 1625 psi | |
BCC Products BC 8660E Urethane Elastomer BC8660E is a multi-purpose elastomer that can perform many functions. Special product characteristics are: excellent use for molds for casting of concrete and plaster, resists moisture absorption, d.. |