Polymer Property : Tensile Strength, Ultimate = 162000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 1120 MPa
162000 psi
Haynes 188 alloy, 40% cold reduction, 3.2 mm thick sheet, 1065°C for 5 minutes
Excellent high temperature strength and very good resistance to oxidizing environments up to 1095°C for prolonged exposure, and excellent resistance to sulfate deposit hot corrosion. Readily fabr..
Tensile Strength, Ultimate 1120 MPa
162000 psi
Special Metals INCONEL® 718SPF™ Nickel Superalloy, Annealed
Typical annealing - continuous process anneal, 1700°F (927°C) at 15 ft (4.57 m) per minute. This produces ASTM No. 12 grain size. Heat capacity, melting range, moduli, and Poisson's ratio re..
Tensile Strength, Ultimate 1117 MPa
162000 psi
Carpenter Custom Age 625 PLUS® Nickel-Base Alloy, Aged 732°C (1350°F)/4hr/AC
Data provided by Carpenter Technology Corporation.Custom Age 625 PLUS® alloy is a precipitation hardenable, nickel-base alloy which, in many environments, displays corrosion resistance similar to t..
Tensile Strength, Ultimate 1120 MPa
162000 psi
ATI Allegheny Ludlum Stainless Steel AL-6XN® Alloy (UNS N08367), 30% Cold Work
The AL-6XN® alloy is a superaustenitic stainless steel which was developed by Allegheny Ludlum Corporation. It exhibits far greater resistance to chloride pitting, crevice corrosion and stress-co..