Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 48.0 - 112 MPa
6960 - 16200 psi
Average value: 86.3 MPa Grade Count:6
Overview of materials for Nylon 6, Film Grade
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Film Grade". Each property range of values reported is minimum and maximum values of appropriat..