Polymer Property : Tensile Strength, Ultimate = 154200 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 1063 MPa
154200 psi
Kennametal Stellite Stellite® 6B solution heat-treated at 1232°C, 15.9 mm thick bar
Machined with tungsten-carbide tools. Inherent wear resistance, resistant to the wearing effects of hard, sharp particles such as in screw conveyors, rock crushing rollers, tile-making machines, and..
Tensile Strength, Ultimate 1063 MPa
154200 psi
40.7% Cold Work
AK Steel NITRONIC® 19-D Duplex Stainless Steel
AK Steel NITRONIC® 19D is a stainless steel with a mixed ferrite and austenite structure. This alloy provides high yield strength (65 ksi minimum {448 MPa}), good drawing and welding characteristi..
Tensile Strength, Ultimate 1063 MPa
154200 psi
Hardened 1800°F, Tempered 1000°F
ATI Allegheny Ludlum 410 Martensitic Stainless Steel
Characteristics: superior wear resistance, hardenable, excellent corrosion resistance. Applications:cutlery, dental and surgical instruments, nozzles, valve parts, hardened steel ball and seats for..
Tensile Strength, Ultimate 1063 MPa
154200 psi
Typical
ATI Allegheny Ludlum Martensitic Stainless Steel Type 410, Hardened + 538°C Temper
Allegheny Ludlum Type 410 is a hardenable straight-chromium stainless steel which combines superior wear resistance of high carbon alloys with the excellent corrosion resistance of chromium stainles..