Polymer Property : Tensile Strength, Ultimate = 15.13 MPa
Polymer Property :
Tensile Strength, Ultimate =
15.13 MPa
Product List
Mechanical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties
Metric
English
Comments
Tensile Strength, Ultimate
15.13
MPa
2194
psi
Vulcanizate, Press cured, TC95 +3min at 160°C
Dow Nordel® IP 4725P High Hardness Extruded Profile
FormulationNordel® IP 4725P