Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 1010 MPa | 147000 psi | Typical |
Kinetics MIM F75 (ASTM F75) HIP Most commonly used within the medical market on applications requiring these characteristics: Bio-compatibility Corrosion resistance High strength Nonmagnetic Wear resistance. Information prov.. |