Kinetics MIM F75 (ASTM F75) HIP

Category Metal , Nonferrous Metal , Cobalt Alloy , Superalloy , Cobalt Base
Manufacturer Kinetics, Inc.
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Kinetics MIM F75 (ASTM F75) HIP.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Most commonly used within the medical market on applications requiring these characteristics: Bio-compatibility Corrosion resistance High strength Nonmagnetic Wear resistance. Information provided by Kinetics, Inc.
Physical Properties Metric English Comments
Density 8.25 g/cc
0.298 lb/in³
Sintered
Mechanical Properties Metric English Comments
Hardness, Rockwell C 25
25
Tensile Strength, Ultimate >= 655 MPa
>= 95000 psi
1010 MPa
147000 psi
Typical
Tensile Strength, Yield >= 448 MPa
>= 65000 psi
558 MPa
81000 psi
Typical
Elongation at Break >= 8.0 %
>= 8.0 %
in 1 inch
30 %
30 %
in 1 inch Typical
Reduction of Area 40 %
40 %
Charpy Impact, Unnotched 176 J
130 ft-lb
1/2 size bar
Component Elements Properties Metric English Comments
Carbon, C <= 0.15 %
<= 0.15 %
Chromium, Cr 26 - 30 %
26 - 30 %
Cobalt, Co 58.85 - 68 %
58.85 - 68 %
Iron, Fe <= 0.75 %
<= 0.75 %
by difference
Manganese, Mn <= 1.0 %
<= 1.0 %
Molybdenum, Mo 5.0 - 7.0 %
5.0 - 7.0 %
Nickel, Ni <= 1.0 %
<= 1.0 %
Nitrogen, N <= 0.25 %
<= 0.25 %
Silicon, Si 1.0 %
1.0 %
Descriptive Properties Value Comments
Surface Finish 40 Ra
Users viewing this material also viewed the following: