Polymer Property : Tensile Strength, Ultimate = 1326 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 9.142 MPa
1326 psi
crosshead speed 20 in./min; ASTM D638
Dow AFFINITY™ SM 1300G Polyolefin Plastomer (POP)
AFFINITY™ SM 1300G is an ethylene alpha-olefin resin for Injection Molding is produced via INSITE™ Technology from Dow Plastics. The resin offers excellent performance in durable injection molded..