Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 8.9997 MPa
1305.3 psi
Dow Corning SILASTIC® 9280/75E KIT PARTS A&B
60 Durometer, 2-part, 1 to 1 mix, translucent, injection moulding grade, Liquid Silicone Rubber.Information provided by Dow Corning
Tensile Strength, Ultimate 8.9997 MPa
1305.3 psi
Dow Corning EG-6301
Two-part, transparent, high modulus (hard) LED encapsulant with high transparency and very long working time.Information provided by Dow Corning
Copyright © lookpolymers.com All Rights Reserved