Material Notes:
60 Durometer, 2-part, 1 to 1 mix, translucent, injection moulding grade, Liquid Silicone Rubber.Information provided by Dow Corning
Physical Properties Metric English Comments
Specific Gravity 1.16 g/cc

@Temperature 25.0 °C
1.16 g/cc

@Temperature 77.0 °F
Solids Content 100 %
100 %
Viscosity 520000 cP
520000 cP
Mechanical Properties Metric English Comments
Hardness, Shore A 74
74
Tensile Strength, Ultimate 8.9997 MPa
1305.3 psi
Elongation at Break 400 %
400 %
Tear Strength 20.02 kN/m
114.2 pli
Compression Set 26 %
26 %
Electrical Properties Metric English Comments
Volume Resistivity 4.80e+15 ohm-cm
4.80e+15 ohm-cm
Processing Properties Metric English Comments
Pot Life 4320 min
4320 min
Shelf Life 15.0 Month
15.0 Month
Descriptive Properties Value Comments
Appearance translucent
Mix Ratio (X:1) 100
Base to Catalyst ETN