Polymer Property : Tensile Strength, Ultimate = 1220 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 8.40 MPa
1220 psi
TPE-0153 (ASTM D 412)
Advanced Elastomer Systems Santoprene® 221-73 W175 Thermoplastic Rubber  (discontinued **)
A colorable thermoplastic UV grade elastomer designed for thin wall extrusion applications with good fluid resistance, formulated to replace thermoset elastomers such as EPDM, polychloroprene, and c..
Tensile Strength, Ultimate 8.38 - 321.27 MPa

@Strain 0.100 - 4.30 %
1220 - 46596 psi

@Strain 0.100 - 4.30 %
Average value: 107 MPa Grade Count:3
Overview of materials for Polyphthalamide (PPA), 50% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 50% Glass Fiber Reinforced". Each property range of values reported is minimum and maxi..
Tensile Strength, Ultimate 8.38 - 321.27 MPa

@Temperature -40.0 - 150 °C
1220 - 46596 psi

@Temperature -40.0 - 302 °F
Average value: 107 MPa Grade Count:3
Overview of materials for Polyphthalamide (PPA), 50% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 50% Glass Fiber Reinforced". Each property range of values reported is minimum and maxi..
Tensile Strength, Ultimate 8.40 MPa
1220 psi
Kuraray HYBRAR® H7125 Hydrogenated Thermoplastic Rubber
Description: HYBRAR® is another in the series of new high performance thermoplastic rubbers developed by KURARAY using their unique isoprene technology. HYBRAR® is a special thermoplastic rubb..
Tensile Strength, Ultimate 8.41 MPa
1220 psi
ASTM D638
Multibase Multi-Flex® A 8406 A Natural TPE Thermoplastic Elastomer
Forms: PelletsProcessing Methods:Injection Molding Information provided by Multibase
Tensile Strength, Ultimate 8.41 MPa
1220 psi
BCC Products BC 4558 Polyester Filler Paste
BC4558 is a unique quickset paste designed for aircraft use in making fast repairs to damaged metal surfaces. Also recommended for use in edge filling honeycomb core and foam core composite panels. ..
Tensile Strength, Ultimate 8.41 MPa
1220 psi
ASTM D412
R70-057 Styrene-based Biomedical Elastomer