Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 12.7 MPa | 1840 psi | Cecilia 20 aged 168 hrs at 175°C |
DuPont Vamac® DP DIAK No. 7 Coagent Test Compound Vamac® DP is an ethylene acrylic dipolymer elastomer. Its general performance characteristics are similar to those of the Vamac® terpolymers, including:Good oil and chemical resistanceHigh temper.. |
|||
Tensile Strength, Ultimate | 12.7 MPa | 1850 psi | 500 mm/min; ASTM D 412 |
Zylog Neoplast® 180 HOFR Thermoplastic Vulcanizate Neoplast 180 HOFR is a flame retardant thermoplastic vulcanizate (TPV) compound, based on polyolefin chemistry, suitable for Injection Molding and Extrusion applications.RoHS Compliant, UV Stabilize.. |
|||
Tensile Strength, Ultimate | 12.7 MPa | 1840 psi | |
Dow DOWLEX™ 2535 Linear Low Density Polyethylene, Narrow MW Distribution DOWLEX® 2535 Polyethylene resin is a narrow molecular weight distribution copolymer designed to offer excellent impact strength and stress crack resistance with good flexibility. It has good proces.. |