Polymer Property : Tensile Strength, Ultimate = 12.2 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 12.2 MPa
1770 psi
ASTM D412-80
DuPont Performance Polymers Hypalon® 20 Chlorosulfonated Polyethylene Rubber, Peroxide Cured Carbon Black Filled Compound
Carbon black compound with 100 parts Hypalon; 40 parts carbon black; 20 parts magnesia; and 5.8 parts Varox® DBPH-50. Physical property data below (except mooney viscosity) are for vulcanizate. Ma..
Tensile Strength, Ultimate 12.2 MPa
1770 psi
ASTM D412
Multibase Multi-Flex® TPE A 3104-8
Multi-Flex TPE contains Kratonâ„¢ G.Data provided by Multibase.
Tensile Strength, Ultimate 12.2 MPa
1770 psi
Cecilia 20 aged 168 hrs at 175°C
DuPont Vamac® DP HVA-2 Coagent Test Compound
Vamac® DP is an ethylene acrylic dipolymer elastomer. Its general performance characteristics are similar to those of the Vamac® terpolymers, including:Good oil and chemical resistanceHigh temper..