Material Notes:
Multi-Flex TPE contains Kratonâ„¢ G.Data provided by Multibase.
Physical Properties Metric English Comments
Density 0.940 g/cc
0.0340 lb/in³
ASTM D792
Linear Mold Shrinkage 0.0137 cm/cm
0.0137 in/in
ASTM D955
Melt Flow 5.0 g/10 min
5.0 g/10 min
(Condition L) ASTM D-1238
Mechanical Properties Metric English Comments
Hardness, Shore D 36
36
10 sec; ASTM D-2240
Tensile Strength, Ultimate 12.2 MPa
1770 psi
ASTM D412
Elongation at Break 600 %
600 %
ASTM D412
Flexural Modulus 0.206 GPa
29.9 ksi
method 1, Proc.B; ASTM D-790
Tear Strength 77.0 kN/m
439 pli
ASTM D624