Polymer Property : Tensile Strength, Ultimate = 1186 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 1186 MPa

@Temperature 177 °C
172000 psi

@Temperature 351 °F
Carpenter Custom Age 625 PLUS® Nickel-Base Alloy, Double Aged 732°C/8hr/FC to 621°C/8hr/AC
Data provided by Carpenter Technology Corporation.Custom Age 625 PLUS® alloy is a precipitation hardenable, nickel-base alloy which, in many environments, displays corrosion resistance similar to t..
Tensile Strength, Ultimate 1186 MPa
172000 psi
57.8% Cold Work
AK Steel NITRONIC® 19-D Duplex Stainless Steel
AK Steel NITRONIC® 19D is a stainless steel with a mixed ferrite and austenite structure. This alloy provides high yield strength (65 ksi minimum {448 MPa}), good drawing and welding characteristi..
Tensile Strength, Ultimate 1186 MPa

@Temperature 316 °C
172000 psi

@Temperature 601 °F
Carpenter Custom 630 (17-Cr-4Ni) Precipitation Hardening Stainless Steel, Condition H 900 (Age-Hardened 482°C/1hr/AC)
Data provided by Carpenter Technology Corporation.Custom 630 (17Cr-4Ni) is a martensitic precipitation/age-hardening stainless steel offering high strength and hardness along with excellent corrosio..