Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 1190 MPa | 172000 psi | Typical |
PSM Industries PolyAlloys MIM-14-4PH Heat Treated Stainless Steel PolyAlloys Injected Metals, a division of PSM Industries, Inc., offers precision, High-Performance components for structural, magnetic and electronic applications that require a high degree of compl.. |
|||
Tensile Strength, Ultimate | 1190 MPa | 172000 psi | |
PSM Industries PolyAlloys MIM-17-4 PH Heat Treated Stainless Steel Information Provided by PolyAlloys, a division of PSM Industries |
|||
Tensile Strength, Ultimate | 1186 MPa @Temperature 177 °C |
172000 psi @Temperature 351 °F |
|
Carpenter Custom Age 625 PLUS® Nickel-Base Alloy, Double Aged 732°C/8hr/FC to 621°C/8hr/AC Data provided by Carpenter Technology Corporation.Custom Age 625 PLUS® alloy is a precipitation hardenable, nickel-base alloy which, in many environments, displays corrosion resistance similar to t.. |
|||
Tensile Strength, Ultimate | 1186 MPa | 172000 psi | 57.8% Cold Work |
AK Steel NITRONIC® 19-D Duplex Stainless Steel AK Steel NITRONIC® 19D is a stainless steel with a mixed ferrite and austenite structure. This alloy provides high yield strength (65 ksi minimum {448 MPa}),
good drawing and welding characteristi.. |
|||
Tensile Strength, Ultimate | 1186 MPa @Temperature 316 °C |
172000 psi @Temperature 601 °F |
|
Carpenter Custom 630 (17-Cr-4Ni) Precipitation Hardening Stainless Steel, Condition H 900 (Age-Hardened 482°C/1hr/AC) Data provided by Carpenter Technology Corporation.Custom 630 (17Cr-4Ni) is a martensitic precipitation/age-hardening stainless steel offering high strength and hardness along with excellent corrosio.. |