Polymer Property : Tensile Strength, Ultimate = 11300 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 78.0 - 117 MPa
11300 - 17000 psi
Average value: 99.0 MPa Grade Count:12
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 20% Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 20% Carbon Fiber Filled". Specific grades with carbon fiber conte..
Tensile Strength, Ultimate 78.0 MPa
11300 psi
ASTM D638
Plenco 6500 Phenolic, Briquette, Injection Molded
PLENCO 06500 is a glass reinforced phenolic molding compound offering improved strength, dimensional stability, and excellent electrical properties. UL recognized under component file E40654. 06500 ..
Tensile Strength, Ultimate 78.0 MPa
11300 psi
ISO 527-2/1A/5
Lubrizol ESTALOC® 59300 Ester-Type, Reinforced Engineering Thermoplastic (European Grade)
Description: Estaloc® RETP (Reinforced Engineering Thermoplastic) is a tough, dimensionally stable, abrasion-resistant thermoplastic that withstands demanding environments. Developed as an extensio..
Tensile Strength, Ultimate 78.0 - 96.0 MPa
11300 - 13900 psi
Dow CYCLOTENE™ 4022-35 Advanced Electronic Resins (PhotoBisbenzocyclobutene BCB)
CYCLOTENE™ 4022-35 advanced electronic resin is I-line-, G-line-, and broad band-sensitive photopolymer that has been developed for use as a dielectric in thin film microelectronic applications.Inf..
Tensile Strength, Ultimate 78.0 - 96.0 MPa
11300 - 13900 psi
Dow CYCLOTENE™ 4024-40 Advanced Electronic Resins (PhotoBisbenzocyclobutene BCB)
CYCLOTENE™ 4024-40 advanced electronic resin is I-line-, G-line-, and broad band-sensitive photopolymer that has been developed for use as a dielectric in thin film microelectronic applications.Inf..
Tensile Strength, Ultimate 78.0 - 96.0 MPa
11300 - 13900 psi
Dow CYCLOTENE™ 4026-46 Advanced Electronic Resins (PhotoBisbenzocyclobutene BCB)
CYCLOTENE™ 4026-46 advanced electronic resin is I-line-, G-line-, and broad band-sensitive photopolymer that has been developed for use as a dielectric in thin film microelectronic applications.Inf..
Tensile Strength, Ultimate 78.0 - 96.0 MPa
11300 - 13900 psi
Dow CYCLOTENE™ XU35075 Advanced Electronic Resins (PhotoBisbenzocyclobutene BCB)
CYCLOTENE™ XU35075 advanced electronic resin is I-line-, G-line-, and broad band-sensitive photopolymer that has been developed for use as a dielectric in thin film microelectronic applications.Inf..
Tensile Strength, Ultimate 78.0 - 96.0 MPa
11300 - 13900 psi
Dow CYCLOTENE™ XU35132 Advanced Electronic Resins (PhotoBisbenzocyclobutene BCB)
CYCLOTENE™ XU35132 advanced electronic resin is I-line-, G-line-, and broad band-sensitive photopolymer that has been developed for use as a dielectric in thin film microelectronic applications.Inf..
Tensile Strength, Ultimate 78.0 - 96.0 MPa
11300 - 13900 psi
Dow CYCLOTENE™ XU35133 Advanced Electronic Resins (PhotoBisbenzocyclobutene BCB)
CYCLOTENE™ XU35133 advanced electronic resin is I-line-, G-line-, and broad band-sensitive photopolymer that has been developed for use as a dielectric in thin film microelectronic applications.Inf..
Tensile Strength, Ultimate 78.0 MPa
11300 psi
5 mm/min
Arkema Group Rilsan® AZM 15 TLD Nylon 12, 15% Glass Fiber Filled (Dry)
Designation ISO 1874-PA12,MHLR,16-030,GF15Rigid grade with glass fiber filler (15%) for injection molding.Available color: natural. Light and heat stabilized. Mold-release agent.Rigidity combined wi..
Tensile Strength, Ultimate 78.0 MPa

@Temperature 982 °C
11300 psi

@Temperature 1800 °F
ATI Allegheny Ludlum 316Ti Austenitic Stainless Steel
Characteristics:excellent resistance to general corrosion, excellent resistance to pitting/crevice corrosion, resistant to sensitization, better creep stress-rupture and tensile strength at elevated..
Tensile Strength, Ultimate 78.0 MPa
11300 psi
ATSM D638
Ashley Polymers Ashlene® 73M Nylon 6, Mineral Reinforced
A mineral reinforced Nylon 6 with improved impact, excellent dimensional stability and heat resistance.Data provided by the manufacturer
Tensile Strength, Ultimate 78.0 MPa
11300 psi
ASTM D638
A. Schulman ComAlloy Hiloy® 638 Nylon 6/6, Mineral Reinforced, Flow Enhanced
Data provided by the manufacturer, ComAlloy International Company.35% Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.