Material Notes:
A mineral reinforced Nylon 6 with improved impact, excellent dimensional stability and heat resistance.Data provided by the manufacturer
Physical Properties Metric English Comments
Density 1.45 g/cc
0.0524 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 78.0 MPa
11300 psi
ATSM D638
Elongation at Break 3.0 %
3.0 %
ASTM D638
Flexural Modulus 4.80 GPa
696 ksi
ASTM D790
Izod Impact, Notched 1.07 J/cm
2.00 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 213 °C
415 °F
ASTM D3418
Deflection Temperature at 1.8 MPa (264 psi) 140 °C
284 °F
ASTM D648