Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 1110 MPa

@Temperature 425 °C
161000 psi

@Temperature 797 °F
Haynes 242® alloy, bar and rings, annealed and aged
Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm..
Tensile Strength, Ultimate 1110 MPa
161000 psi
HP Alloys Alloy X, 30% Cold Worked
30% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc., Allvac, and Haynes International.
Tensile Strength, Ultimate >= 1110 MPa
>= 161000 psi
TIMET TIMETAL® 679 (Ti-11Sn-5Zr-2.25Al-1Mo-0.2Si) Titanium Alloy; Quenched & Aged
High-Temperature, High-Strength Creep Resistant AlloyIndustry Specifications: USA Aerospace: AMS 4974.Features: TIMETAL 679 has excellent tensile strength and is creep resistant up to 450°C. It i..
Tensile Strength, Ultimate 1110 MPa
161000 psi
Longitudinal
AK Steel 15-5 PH® Precipitation Hardening Stainless Steel, Condition A
AK Steel 15-5 PH® provides high strength, good corrosion resistance, good mechanical properties at temperatures up to 600°F (316°C), and good toughness in both base metal and welds. Short-time, ..
Tensile Strength, Ultimate 1110 MPa
161000 psi
Carpenter Gall-Tough® Stainless
Data provided by Carpenter Technology Corporation.6.4 mm diameter tensile specimens from center of 25.4 mm diameter bar annealed 1066°C 1 hour, water quenched, and ground.Threshold Galling Stress 1..
Tensile Strength, Ultimate 1110 MPa

@Temperature 205 °C
161000 psi

@Temperature 401 °F
Haynes 242® alloy, hot rolled plate, annealed and aged
Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good thermal..
Tensile Strength, Ultimate 1110 MPa
161000 psi
Haynes 25 alloy, room temperature after 15% cold reduction, 1120°C anneal for 5 minutes
Excellent high-temperature strength with good resistance to oxidizing environments up to 980°C for prolonged exposures and excellent resistance to sulfidation and excellent resistance to metal gall..
Copyright © lookpolymers.com All Rights Reserved