Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 699.8 MPa | 101500 psi | |
Special Metals INCONEL® 690 Nickel Superalloy, Cold Drawn Tube, 0.75 inch (19.0 mm) o.d. and 0.065 inch (1.65 mm) Thickness Composition adjustments for nuclear applications: 28-31 Cr; 0.04 max C; 0.10 max Co.Tensile strength (ultimate and yield) and elongation values reported here are typical for Cold Drawn Tube, 0.75 in.. |