Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Strength, Ultimate = 1.96 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 1.96 MPa
284 psi
JIS K6301
Stellarchem GP-975B TPE Compound
This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete..
Tensile Strength, Ultimate 1.96 MPa

@Time 605000 sec
284 psi

@Time 168 hour
Heat Aging; ASTM D 412/ASTM D 573
Zylog Neoplast® 135 FT EB Thermoplastic Vulcanizate
Neoplast 135 FT EB is a soft, dynamically vulcanized thermoplastic vulcanizate (TPV), based on polyolefin chemistry, and is intended for Injection Molding and Extrusion applications.RoHS Compliant, ..
Copyright © lookpolymers.com All Rights Reserved