Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 1.40 - 51.0 MPa

@Temperature -20.0 - 49.0 °C
203 - 7400 psi

@Temperature -4.00 - 120 °F
Average value: 19.8 MPa Grade Count:11
Overview of materials for Ethylene Vinyl Acetate Copolymer (EVA), Molded/Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Vinyl Acetate; Molded/Extruded". Each property range of values reported is minimum and maximum ..
Tensile Strength, Ultimate 1.40 MPa

@Temperature 49.0 °C
203 psi

@Temperature 120 °F
Type IV, crosshead speed 2 in/min; ASTM D638
DuPont Elvax® 250 Ethylene-Vinyl Acetate Copolymer Resin