Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 0.0689 MPa | 10.0 psi | TM R050-36 |
Resinlab® UR3001HP Black Urethane Encapsulant Resinlab™ UR3001HP Black is a black, two component, room temperature curing urethane encapsulating system. It is designed to cure completely at room temperature. UR3001HP Black provides excellent e.. |
|||
Tensile Strength, Ultimate | 0.0689 - 29.0 MPa | 10.0 - 4210 psi | Average value: 9.80 MPa Grade Count:58 |
Overview of materials for Thermoset Polyurethane, Adhesive This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Polyurethane, Adhesive". Each property range of values reported is minimum and maximum values .. |
|||
Tensile Strength, Ultimate | 0.0689 MPa | 10.0 psi | TM R050-36 |
Resinlab® UR3001HP Clear Urethane Encapsulant Resinlab™ UR3001HP Clear is a clear, two component, room temperature curing urethane encapsulating system. It is designed to cure completely at room temperature. UR3001HP Clear provides excellent e.. |