Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Falling Dart Impact | 13.0 J | 9.59 ft-lb | ASTM D3763 |
LNP Thermocomp® SF-1006 Polyamide 12, Glass Fiber Reinforcement
(discontinued **) Forms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still active under new names.. |