Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Falling Dart Impact | 12.0 J | 8.85 ft-lb | ASTM D3763 |
LNP Thermocomp® STN-F-1006 HS Polyamide 46, Glass Fiber Reinforcement
(discontinued **) Features: Heat StabilizedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are sti.. |