Polymer Property : Falling Dart Impact = 8.50 J Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Falling Dart Impact 8.50 J
6.27 ft-lb
ASTM D3763
LNP Stat-Kon® PDX-E-99550 CCS Polyetherimide, Carbon Fiber Reinforcement  (discontinued **)
Features: Low to None Ion Content, Electrically ConductiveForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued..
Falling Dart Impact 8.50 - 11.8 J
6.27 - 8.70 ft-lb
Average value: 9.88 J Grade Count:4
Overview of materials for Nylon 610
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 610". Each property range of values reported is minimum and maximum values of appropriate MatWeb e..
Falling Dart Impact 8.50 - 11.8 J
6.27 - 8.70 ft-lb
Average value: 9.88 J Grade Count:4
Overview of materials for Nylon 610, Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 610, Glass Reinforced". Each property range of values reported is minimum and maximum values of ap..
Falling Dart Impact 8.50 J
6.27 ft-lb
ASTM D3763
LNP Lubricomp® QFL-4036 BK8-115 Polyamide 6/10 Copolymer, Glass Fiber Reinforcement, PTFE Lubricant  (disconti
Features: LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still ac..