Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Falling Dart Impact | 7.62 J | 5.62 ft-lb | ASTM D3763 |
LNP Thermocomp® LC-1006 EM Polyetheretherketone, Carbon Fiber Reinforcement
(discontinued **) Features: Good MoldabilityForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are st.. |