Polymer Property : Falling Dart Impact = 59.6561 J Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Falling Dart Impact 59.6561 - 59.6561 J

@Temperature -28.9 - -28.9 °C
44.0001 - 44.0001 ft-lb

@Temperature -20.0 - -20.0 °F
Average value: 59.7 J Grade Count:1
Overview of materials for Polycarbonate, Impact Modified
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Impact Modified". Each property range of values reported is minimum and maximum values of..