Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Falling Dart Impact | 59.6561 - 59.6561 J @Temperature -28.9 - -28.9 °C |
44.0001 - 44.0001 ft-lb @Temperature -20.0 - -20.0 °F |
Average value: 59.7 J Grade Count:1 |
Overview of materials for Polycarbonate, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Impact Modified". Each property range of values reported is minimum and maximum values of.. |