Polymer Property : Falling Dart Impact = 542 J Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Falling Dart Impact 542 J

@Temperature -40.0 °C
400 ft-lb

@Temperature -40.0 °F
ASTM D1709A
Spartech PETG 3D Lenticular 3-D Specialty Sheet
Description: Specialty SheetInformation provided by Spartech.
Falling Dart Impact 542 J

@Temperature -40.0 °C
400 ft-lb

@Temperature -40.0 °F
ASTM D1709A
Spartech APET SP4110 Copolyester Sheet
Description: Copolyester SheetInformation provided by Spartech.