Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Falling Dart Impact | 32.5397 - 176.257 J @Temperature -40.0 - -40.0 °C |
24.0000 - 130.000 ft-lb @Temperature -40.0 - -40.0 °F |
Average value: 104 J Grade Count:2 |
Overview of materials for High Density Polyethylene (HDPE), Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Impact Grade". Each property range of values reported is minimum and m.. |
|||
Falling Dart Impact | 31.1839 - 176.257 J @Temperature -40.0 - -40.0 °C |
23.0000 - 130.000 ft-lb @Temperature -40.0 - -40.0 °F |
Average value: 125 J Grade Count:3 |
Overview of materials for High Density Polyethylene (HDPE), Injection Molded This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Injection Molded". Each property range of values reported is minimum a.. |